Most of a welded part's cost is set on the drawing board long before the first spark. The number, size, accessibility and distortion tendency of welds are decided in design. The rules below are a checklist for buyers and designers before a drawing goes to a supplier.
1. Think About Weld Access
The torch or electrode must reach the joint at the right angle. Welds in tight corners, between nested plates or inside closed boxes are either impossible or poor. Checking in the 3D model with the torch body in mind is a good start.
2. Size Welds by Calculation
Doubling the throat size of a fillet weld roughly quadruples weld metal volume. Oversized welds "to be safe" increase both cost and distortion.
3. Reduce the Number of Welds
A bent sheet can replace two plates welded together. A contour laser-cut in one piece is cheaper and cleaner than welding several small parts.
4. Build in Symmetry
Welds balanced around the neutral axis offset each other's distortion. Heavy welding on one side pulls the part that way (see weld distortion).
5. Avoid Intersecting Welds
Points where three welds meet concentrate stress and defects. Corner copes (scallops) separating the welds improve quality and fatigue life.
6. Keep Away From High-Stress Zones
Move welds away from sections of maximum bending stress and abrupt changes in section where possible. On fatigue-loaded parts this directly affects the FAT class.
7. Use Standard Material and Sections
Readily available plate thicknesses and sections shorten lead time. A special thickness or rare grade can hold up the whole order for one part.
8. Allow Flat-Position Welding
Flat and horizontal positions are fastest and give the best quality. If the part can be turned over or rotated on a positioner, overhead and vertical welding is reduced.
9. Tolerance by Function
Leave tight dimensions that welding cannot hold to post-weld machining and define machining allowance. On non-functional faces, ISO 13920 general tolerances are enough.
10. Plan Surface Treatment From the Start
Drain holes in closed sections going to galvanising or e-coat, seal welds or gaps at laps, and rounded edges for painting belong in the design.
Early Design Review
When sending a drawing to a supplier, asking "what would you change to make this cheaper and better?" is often the most productive price discussion.
At ArmaWeld: at quotation we review drawings for weld access, weld size, distortion and surface treatment, and send change proposals that affect cost and quality with the quote. The final decision always rests with the design owner. Build-to-print manufacturing →
Frequently Asked Questions
Where is a welded part's cost mostly set?
In design: number, size and accessibility of welds.
What happens if throat size grows?
Doubling the throat roughly quadruples weld metal.
Why are intersecting welds a problem?
Stress and defects concentrate; separate them with copes.
What should you ask the supplier?
What design change would lower cost and raise quality.
Let us review your drawing for manufacturability
Send drawings; we will prepare our quote with proposals.
Request a Quote →