A cable duct on a chassis, a cover on a panel, a hose clamp on a housing. Thin sheet cannot be tapped; there is no access behind to hold a nut. The answer is to weld a fastener to the part: a stud or a weld nut. Chosen wrongly, the result is studs breaking off in the field and threads full of paint.

Stud Welding (ISO 14555)

  • Drawn-arc stud welding (ceramic ferrule or shielding gas): a short arc forms between stud and part, then the stud is plunged into the molten pool. Suits larger studs and load-bearing connections; fusion across the full section.
  • Short-cycle drawn arc: for smaller diameters and medium sheet thickness.
  • Capacitor discharge (CD): a very short energy discharge. Ideal for small studs on thin sheet without marking the reverse side; preferred on painted or visible faces. Load capacity is limited.

Weld Nuts

  • DIN 929 hex and DIN 928 square weld nuts: projections allow resistance (projection) welding to sheet. Fast and repeatable in series; common in automotive and sheet assemblies.
  • MAG-welded nuts: on thick parts or low volumes without projection equipment, the nut is welded around its perimeter. Heat can distort the thread; a thread check or retapping may be needed.

Common Problems

  • Spatter and paint in the thread: protect threads during welding and painting; plan plugs, masking or post-paint tapping.
  • Wrong position: secure hole and stud positions with a fixture (see welding fixtures).
  • Marks or burn-through on the reverse: choose the method carefully on thin, visible sheet.
  • Coatings: zinc on galvanised sheet affects the weld; suitable parameters or method are needed.

Testing

ISO 14555 defines pre-production and production tests for stud welding: bend test (bending the stud with a hammer to a set angle), tensile or torque test and visual inspection. For weld nuts, push-out and torque tests are common. Test frequency belongs in the specification.

What to State on the Drawing

Stud or nut type and standard, material, position tolerance, thread protection, test method and frequency, and whether it is applied before or after coating.

At ArmaWeld: for MAG-welded nuts and fasteners we secure position with fixtures and protect threads during welding and painting. Where stud or projection welding is required, we define the method at quotation and coordinate with partners if needed. Build-to-print manufacturing →

Frequently Asked Questions

Which standard covers stud welding?

ISO 14555; it defines methods and tests.

Which method for thin sheet?

Usually capacitor discharge, to avoid marking the reverse side.

How are weld nuts attached?

By projection welding in series, by MAG around the perimeter at low volumes.

What if paint fills the thread?

Plan masking or post-paint tapping in advance.

Welded parts with fastening points?

Send drawings; we will propose the method and prepare our quote.

Request a Quote →