Every kilogram taken out of a trailer chassis is added to payload. Lightening a crane boom affects lifting capacity; lightening an agricultural machine affects fuel use and soil compaction. Weight reduction is therefore product performance, not just material saving. In welded construction, however, every method has consequences for fabrication and strength.
1. High-Strength Steel
Moving from S355 to steels with higher yield strength such as S700 or S960 allows thinner plate for the same load. But:
- Welding requires strict control of heat input and cooling time (t8/5); exceed it and the HAZ softens.
- Fatigue strength at the weld does not rise with steel grade. On fatigue-loaded parts, lightweighting must go hand in hand with better weld details.
- On thin plate, buckling and stiffness may govern; strength may suffice while deflection grows.
- Material supply and filler selection need more care.
2. Section Choice
For members in torsion, closed box sections give far higher torsional stiffness than open sections (U, I) at the same weight. On fabricated girders, web and flange thickness can vary along the length with the load (see fabricated girders).
3. Cut-Outs and Laser Cutting
Laser-cut lightening holes in low-stress webs reduce weight and provide routing for cables and hoses. Hole edges and corner radii must be designed to avoid stress concentration.
4. Bent Profiles and Fewer Welds
Bent sheet profiles replace several welded plates, reducing weld metal and distortion. Sizing welds by calculation avoids unnecessary weld metal and heat.
5. Welded Instead of Cast
Converting heavy castings to welded construction can save weight with thin plates placed where needed (see welded instead of cast).
Points to Watch
- Lightweighting proposals must be verified by calculation or test; the supplier proposes from a fabrication standpoint, structural responsibility stays with the design owner.
- Thinner plate can increase weld distortion; fixtures and weld sequence become more important.
- High-strength steels need larger bend radii; involve the bending partner early.
At ArmaWeld: in lightweighting projects we assess the fabrication side: heat-input control on high-strength steels, weld sizes, and reducing welds through cutting and bending. Cutting and bending are coordinated with our partners; structural approval always rests with the design owner. Machine frame fabrication →
Frequently Asked Questions
Does high-strength steel always save weight?
Under static load yes; if fatigue or stiffness governs, the gain may be limited.
Does weld fatigue strength rise with steel grade?
No; without better weld details there is no fatigue gain.
Which section suits torsion?
Closed box sections are far stiffer at the same weight.
Who approves lightweighting?
Structural responsibility lies with the design owner; the supplier proposes fabrication changes.
Lightweight welded structures?
Send drawings and targets; we will quote with fabrication proposals.
Request a Quote →