EN ISO 3834-2

Certified welding for heavy steel.

Qualified welders and approved WPS, built exactly to drawing.

EN 1090-2 · EXC3

Big parts, no compromise.

Booms, chassis and load-bearing parts. Approved weld procedures for every grade, from S235 to Strenx 1100.

NDT · Reported delivery

Every seam inspected.

VT, PT, MT and UT done in house. Every part ships with its inspection report.

Every weld bears
an engineer's
signature.

EN 1090-2, EN ISO 3834-2, ISO 9001, ISO 14001 and ISO 45001 certified welded fabrication and NDT. From S235 to Strenx 1100, approved WPS and certified welders for every steel group.

WELDED FABRICATION ◆ PLATE CUTTING ◆ BENDING & FORMING ◆ CRANE MANUFACTURING ◆ PRESSURE VESSELS ◆ CONSTRUCTION MACHINERY BODY ◆ TANKS ◆ NDT / NON-DESTRUCTIVE TESTING ◆ HARDOX · Strenx · RAEX · S690 ◆
ArmaWeld · WELDED FABRICATION EN 1090-2 · EN ISO 3834-2 · ISO 9001 · 14001 · 45001 KONYA · TR
EN 1090EXC3
Execution Class Capability
EN ISO3834-2
Comprehensive Quality
100%
Part-level Traceability
S235–Strenx 1100 · HARDOX · Al
Specialist Steel Grades
■ WPS–142 · FILLET WELD
MAG 135 / G3Si1
a = 6 mm · L = 220 mm
EN ISO 9606-1
VOLTAGE · V
28.4 V
WIRE FEED
7.8 m/dk
From the shop floor

See the work.

Hover over a card to play the video Scroll and the videos play on their own
01 / Who it is for

A clear process for technical decision-makers.

02 / Who we serve

OEMs, EPCs and fabrication partners.

Machinery & Equipment OEM

Serial and prototype welded fabrication for bodies, buckets, booms and wear parts.

Energy & Process Plants

Pressure vessels, platforms and steel structures — documented production under PED and EN 1090.

Structure & Infrastructure Contractors

EXC3 structural steel, assembly support and site-ready part kits.

New equipment

Our 35 m submerged arc welder is now in production.

Submerged arc welding for long linear seams, booms and chassis, in one set-up with repeatable quality.

Linear seams Booms Chassis
Submerged Arc Welding →
03 / Services

SVC — 001 / 008

We manage metal processing with engineering discipline from end to end.

01

Welded Fabrication

MIG/MAG · 135 TIG · 141 FCAW · 136 EN ISO 3834-2 WPQR Qualified

From S235 to Strenx 1100, S690QL and S960QL to HARDOX — reliable production across every steel group including stainless and aluminium with approved WPS.

↗
02

Sheet Cutting & Profile Processing

CNC Plazma Lazer Giyotin Profil Testere

Carbon steel, stainless, Hardox, Strenx and aluminium — tolerance-controlled cutting and weld-ready preparation to technical drawing.

↗
03

Bending & Forming

Abkant Pres · 200 t Silindir ±0.5° Hassasiyet

V-bending, U-forming and cylindrical shaping — programmed angle, radius and assembly-fit management.

↗
04

Mechanical Assembly & Shipment Prep

ISO 898 Cl.8.8/10.9 Dijital Tork Lazer Hizalama

Sub-assembly, torque recording and functional testing — shipment packaging integrated into the project plan.

↗
05

NDT & Non-Destructive Testing

VT · PT · MT · UT EN ISO 9712 L2 RT Partner Lab

4 inspection methods in-house, EN ISO 5817 Class B acceptance — every weld documented, no record omitted.

↗
06

Construction Machine Body & Bucket

HARDOX 400/450/500 Strenx 700/960 RAEX Series Production

Bucket, bowl, blade and body fabrication in wear steels — serial production fixtures and MT inspection included.

↗
07

Crane Construction

EN 1090 EXC2 CE Marking 1 – 20 t

Overhead bridge, jib and monorail crane structure fabrication — delivered with FEM static calculation and CE DoP.

↗
08

Pressure Vessels & Process Tanks

PED Cat. I–II RT/UT %100 P265GH · 304L · 316L

Storage tanks, reaction vessels and heat exchangers under PED Cat. I–II — complete document package with RT + UT + CE declaration.

↗
Beyond the job shop

One contact, one responsibility in your supply chain.

Working with ArmaWeld doesn't add another supplier to your list — it takes an entire burden off your supply chain.

TopicConventional job shopArmaWeld
ContactSeparate firms for cutting, forming, welding and inspection✓ One contact; ArmaWeld manages the chain
Weld qualityDepends on the craftsman✓ Procedure-driven: approved WPS/WPQR and certified welders
InspectionOutsourced, if at all✓ Planned NDT by Level 2 personnel · acceptance EN ISO 5817 B
DocumentsOn request, often incomplete✓ Complete document file with every delivery
Order statusAsked by phone✓ Live in the portal, 24/7
EngineeringBuilt exactly as drawn✓ With manufacturability and cost proposals
FlexibilityMinimum order quantity✓ No quantity threshold, from prototype to series
04 / Traceability Process

TRC — SOP.001

Raw material to delivery;
7 steps,
zero blind spots.

At ArmaWeld every work order opens with a digital serial number; heat number, WPS, welder, NDT report, dimensional check and shipping document all accumulate in the same record. Hover over the steps below to inspect any point in the production journey.

JOB-A142 / SER-0142

Track your order live.

View production stages, operator records and download technical documents from the customer portal.

Customer Portal Login
Customer portal

Every stage of your order, on one screen, in real time.

When you approve a quotation, a dedicated portal account is opened for you. Fed by real production data, it lets your purchasing, quality and engineering teams see the same record. Not phone traffic — a single source of truth.

portal.armaweld.com
ArmaWeld customer portal screen: Dashboard
The moment you log in, a summary of all your orders is in front of you. Actual portal screens · demo account data

Dashboard

Open, in-production and completed orders, plus delivery performance, at a glance.

Live order tracking

Where your order stands on the 7-stage line, in real time.

Traceability timeline

Operator, date, notes and documents at every stage.

Quality documents

WPS, WPQR, 3.1, NDT and CE / DoP documents as signed PDFs.

Lead time & performance

Estimated delivery, monthly deliveries, on-time delivery rate.

Notifications & messages

Stage and document notifications; every conversation linked to its job.

Quote requests from the portal

Upload DWG / DXF / PDF and follow the quotation process live.

After-sales

Installed products, spare parts, service and warranty requests.

Who gains what from the portal?

Purchasing

Sees lead-time risk early and plans on real data.

Quality / Engineering

Reviews and approves WPS, NDT and dimensional reports before shipment.

Management / Audit

Manages the supplier on evidence; presents documents from the archive in one click during audits.

TLS-encrypted connection · role-based access · regular backups · covered by a confidentiality agreement.

Explore the portal screen by screen →
0metres
Weld Seam / 2026 Q1
Live workshop data · MIG+TIG+E-ARC total
0%
Traceability Rate
Every part recorded with serial number
0%
NDT Rejection Rate
≈65% below industry average
0hours
Avg. Quote Turnaround
After technical drawing submission
05 / Welding Process Comparator

PROC — 111 · 135 · 141

Which arc for which job? Technical facts at a glance.

MIG
MAG
ISO 4063
PROSES 135 / 136
Gas Metal Arc Welding — Metal Inert / Active Gas
  • CurrentDC / 120–320 A
  • Voltage18–32 V
  • Gas%82 Ar + %18 CO₂
  • Wire Dia.0.8 – 1.6 mm
  • Efficiency≈ %95
  • MaterialCarbon st., stainless, Al

High deposition rate, long welds, series production, construction machinery, crane structures and structural steel — first choice.

Speed
9.2
Precision
7.0
Cleanliness
7.2
TIG
ISO 4063
PROSES 141
Gas Tungsten Arc Welding — Inert Gas
  • CurrentAC / DC · 20–220 A
  • Voltage10–18 V
  • Gas100% argon (He addition)
  • ElectrodeWT20 / WC20, 1.6–3.2 mm
  • Efficiency≈ %100
  • MaterialPaslanmaz, Alm, Ti, Ni.

Thin wall, precise root passes, stainless tanks & pressure vessels, hygienic food applications, visible welds — indispensable.

Speed
4.5
Precision
9.8
Cleanliness
9.8
E-ARC
ISO 4063
PROSES 111
Shielded Metal Arc Welding — SMAW
  • CurrentAC / DC · 60–300 A
  • Voltage20–34 V
  • GasNone (from coating)
  • ElectrodeBasic / rutile, 2.5–5.0 mm
  • Efficiency≈ %65
  • MaterialSite steel, high C

Site conditions, outdoor, wind-exposed jobsites and repair welds — robust and reliable; no gas required.

Speed
5.8
Precision
6.2
Cleanliness
5.0
All Method Details →
06 / Document Sample

DOC — WPS.142-A

Every delivery includes a dossier: WPS, WPQR, NDT, Tracking.

We don't just deliver parts — alongside every shipment we deliver a complete document dossier proving how the part was manufactured, by whom it was welded, what raw material was used and which inspections it passed.

  • WPS — Welding Procedure SpecificationPDF · Signed
  • WPQR — Procedure Qualification RecordEN ISO 15614
  • Welder Qualification CertificatesEN ISO 9606
  • Raw Material Test Certificates (3.1)EN 10204
  • NDT Reports (VT / PT / UT)EN ISO 17637
  • Dimensional Inspection ReportEN ISO 13920
  • CE Declaration of Conformity (if required)EN 1090-2
View Document Package →

WELDING PROCEDURE SPECIFICATION

WELDING PROCEDURE SPECIFICATION · EN ISO 15609-1
ArmaWeld
WPS No
WPS-142-A
Revision
Rev.02 / 2026-03-14
WPQR Ref.
WPQR-142 / NB-approved
Process
135 (MAG) + 141 (TIG root)
Material
S355J2+N / Group 1.2
Thickness
t = 12 mm
Joint Type
BW / Butt Weld
Position
PA · PB · PF
Pass Process Ø (mm) Current (A) Voltage (V) Speed (cm/min)
Root1412.411012.49
Fill-11351.222024.832
Fill-21351.224026.430
Cap1351.221023.228
Shielding Gas
M21 · %82 Ar + %18 CO₂
Preheat
Tp ≥ 20 °C
Welding Engineer
IWE · Ali Eren
Approval
14 / 03 / 2026
ARMAWELD
APPROVED
QUALITY
07 / Sectors

IND — 001 / 008

Present wherever critical load is carried in heavy industry.

References

CLT — REFERANS

From welded fabrication to NDT reports, single accountability chain.

■ EARTHMOVING MACHINERY / HARDOX · Strenx · S700MC ■ STRUCTURAL STEEL / S355 · S690QL · Strenx ■ ENERGY / SOLAR / S275 · HDG ■ RAIL / EN 15085 CL1 ■ PROCESS / PRESSURE VESSELS / PED · RT %100
"

Previous suppliers welding S960QL skipped preheat — we had cracks. At ArmaWeld the WPS and preheat protocol were complete.

PROCUREMENT MGR · HEAVY VEHICLE OEM
"

We requested the EN 1090 EXC3 document package. CE dossier, WPQR list, NDT records — all ready on first delivery.

QUALITY ENGINEER · ENERGY PLANT
"

We have placed serial bucket orders every year for three years. Per-part quality variation is near zero — that discipline is hard to maintain.

GENERAL MANAGER · MACHINERY MANUFACTURING
View All Projects →
08 / Technical insights

Welding engineering notes.

09 / Certifications

The document backbone of auditable production.

Every project is built on approved WPS, certified personnel and traceable quality records. The standards below are actively maintained.

01Active

EN 1090-2 EXC3

Structural steel · CE marking

Factory production control and EXC3 execution class for load-bearing steel fabrication; DoP and technical file delivery.

02Active

EN ISO 3834-2

Welding quality system

Welding quality framework covering WPS, WPQR, welder qualification and full traceability chain.

03Active

ISO 9001:2015

Quality management system

Corporate quality system built on process management, customer focus and continuous improvement.

04Active

ISO 14001:2015

Environmental management system

Certified environmental management covering waste handling, resource efficiency and environmental impact control.

05Active

ISO 45001:2018

Occupational health & safety

Certified OH&S management system with risk assessment, PPE management and site audits.

06Active

EN ISO 9712

NDT Level 2 personnel

In-house Level 2 certified team performing VT, PT, MT and UT inspections.

07Active

EN ISO 9606-1

Certified welder workforce

Welder qualifications for MAG, TIG and MMA by material group and welding position.

08

View all documents

Document pack

Certificates, sample WPS/WPQR and the delivery file on our quality page.

Engineering Tools

Technical calculators and project checklist.

Heat input, preheat estimate, sector-based material recommendation and document checklist — a quick start for WPS preparation.

Open all tools →
Let's Work Together

Send your drawings — quote within 48 hours.

We review your DWG/DXF/PDF files and provide a comprehensive price quote including the welding method, material grade, applicable WPS and NDT plan.

Quote Form View Our Projects